Alumina Ceramic Foam Tace don Narkakken aluminum gami tacewa

Alumina Ceramic Foam Tace don Narkakken aluminum gami tacewa

Takaitaccen Bayani:

Alumina Foam ceramics foundry filter ana amfani dashi galibi don tacewa na aluminium da aluminium a cikin kafuwa da gidajen simintin.Tare da kyakkyawan juriyar girgizawar thermal da juriyar lalata daga gurɓataccen aluminium, za su iya kawar da inclusions yadda ya kamata, rage iskar gas da kuma samar da kwararar laminar, sannan ƙarfen da aka tace yana da tsabta sosai.Ƙarfe mafi tsafta yana haifar da mafi kyawun simintin gyare-gyare, ƙarancin tarkace, da ƙarancin haɗakarwa, duk waɗannan suna ba da gudummawa ga ribar ƙasa.


Cikakken Bayani

Tags samfurin

Ƙayyadaddun bayanai don tacewa yumburan yumbura

Girma (mm)

Girma (inch)

Yawan zuba (kg/s)

Iyawar tacewa (ton)

178*178*50

7*7*2

0.2-0.6

5

228*228*50

9*9*2

0.3-1.0

10

305*305*50

12*12*2

0.8-2.5

15

381*381*50

15*15*2

2.2-4.5

25

430*430*50

17*17*2

3.0-5.5

35

508*508*50

20*20*2

4.0-6.5

45

585*585*50

23*23*2

5.0-8.6

60

Kaddarorin jiki & sunadarai

Kayan abu

Alumina

Launi

Fari

Girman Pore

8-60 ppi

Porosity

80-90%

Refractoriness

≤1200ºC

Karfin Lankwasawa

> 0.6Mpa

Ƙarfin Matsi

> 0.8Mpa

Girma-nauyin

0.3-0.45g/cm3

Thermal girgiza juriya

6 sau/1100ºC

Aikace-aikace

Aluminium, Aluminum gami da sauran abubuwan da ba na ƙarfe ba

Ayyuka

1. Kazantar da ruwan ƙarfe mai narkewa
2. Sauƙaƙe tsarin gating
3. Inganta tsarin ƙarfe na simintin gyaran kafa
4. Rage simintin gyare-gyare
5. Inganta ƙimar simintin gyare-gyare
6. Rage lahani na sake-oxidation na ciki
7. Rage lahanin saman bayan yin aikin simintin gyaran kafa

Amfani

1.Yawan Ruwa
Cire abubuwan da aka haɗa suna sa ƙarfe ya zama ruwan sama, yana haifar da sauƙin cika ƙura, mafi kyawun tsarin simintin, da mafi kyawun simintin sashe na bakin ciki.

2. Rage Mold da Mutuwa
Cire abubuwan da aka haɗa da sauran tarkace marasa ƙarfe daga narke yana rage mu'amalar ƙura da ƙura, wanda ke ƙasƙantar da yanayin ƙura da rayuwar sabis.

3.Longer Tool Life
Oxide har ma da haɗaɗɗun tsaka-tsaki suna haifar da "masu wuya" waɗanda ke lalata kayan aiki a cikin injina da kammala ayyukan.Tacewa yana rage lalacewa na kayan aiki kuma yana ƙara yawan aiki.

4. Kadan ya ƙi
Inclusions nucleate porosity, haifar da zafi hawaye a lokacin solidification, haifar da lahani da cewa mar bayyanar, da kuma sau da yawa rage inji Properties.A yawancin lokuta, tacewa yana ƙi daga irin waɗannan dalilai zuwa kusan sifili.Inganta yawan amfanin ƙasa zuwa kusan 100% da rage ƙin ƙimar zuwa kusan 0% na gama gari.

Aikace-aikace

1. Yashi
2. Harsashi
3. Mutuwar ƙarancin matsi
4. Dindindin simintin gyare-gyare
5. Riƙewa da tsarin canja wuri